ebpvd的特点:生产率高、均匀性差、不稳定,金属蒸汽的控制是一个难题,沉积过程会形成缺陷,影响镀层的均匀性。 feature of ebpvd:high productivity ,poor uniformity , not stable .metal vapor control is a difficult problem. defects will come in the process of deposition and affect the uniformity of the coating. right?
2013-06-16 569阅读
问题/讨论
回复(5)
我要向AI提问
AI回答:
Yes, that is correct. The translation of the technical equipment conference record is accurate. It states that the features of EBPVD (Electron Beam Physical Vapor Deposition) include high productivity, poor uniformity, and instability. The control of metal vapor is a challenging task, and the deposition process can lead to defects that affect the uniformity of the coating.
2023-07-01
追问:
  • Luu.Van.Dung
    what's more,if the carbide fiber breaks in magnetron sputtering, it would lead to short circuit and the device wouldn't work. 不知怎么样,楼主参考一下
    2013-06-18
  • Alexander
    谢谢,我就是要这样简单明了的,第一次翻译这种文件,长经验了。
    2013-06-19
  • bruce5
    unstable, hard vapor control
    2013-06-18
  • lily35
    Besides,in a magnetron sputtering,If the silicon carbide fiber he a breakage,it would easily caused to short circuit,resulting in  a unnormal operation.
    2013-06-17
  • Mei.Hong
    此外,在磁控溅射中,如果碳化硅纤维断裂,容易引起短路,设备就无法正常运转。
    If the silicon carbide fiber he a breakage,which would easily caused to short circuit,equipment will not he a normal operation.

    right?